Description
|
The functionalization of thin, flexible glass with piezoelectric oxides is a pathway toward transparent electromechanical devices. The crystallization of lead zirconate titanate thin films on thick, rigid glass is previously demonstrated using flash lamp annealing to selectively anneal the films, without damaging the substrates. In this work, a 2-step process suitable for Schott AF 32 eco glass and Corning Willow glass is developed, both 100 μm thick, the latter of which is compatible with roll-to-roll processes. Herein, demonstration is done of: 1) the importance of heat management during flash lamp annealing; and 2) a method to orient perovskite thin films during their crystallization by flash lamp annealing. With this process, the 540 nm thick lead zirconate titanate thin films with morphotropic phase boundary composition display a relative permittivity εr of 330, a dielectric loss of 8.4% and a piezoelectric coefficient (Formula presented.) of 5.5 C m−2. This work demonstrates the feasibility of transparent piezoelectric films, which has a potential to opening the way to flexible and invisible devices. (2025-06-20)
***This entry has been automatically imported via OpenAlex by LIST harvest scripts. Please refer to https://doi.org/10.1002/smsc.202500227 for the original and latest version of the publication*** (2026-07-01)
|
|
Keyword
|
Materials science, Lead zirconate titanate, Annealing (glass), Thin film, Crystallization, Piezoelectricity, Composite material, Dielectric, Optoelectronics, Phase boundary, Phase (matter), Ferroelectricity, Nanotechnology, Chemical engineering |